dc.contributor.authorMacková, A.
dc.contributor.authorFernandes, S.
dc.contributor.authorMatejíček, J.
dc.contributor.authorVilémová, M.
dc.contributor.authorHolý, V.
dc.contributor.authorLiedke, M.O.
dc.contributor.authorMartan, Jiří
dc.contributor.authorVronka, M.
dc.contributor.authorPotoček, M.
dc.contributor.authorBábor, P.
dc.contributor.authorButterling, M.
dc.contributor.authorAttallah, A.G.
dc.contributor.authorHirschmann, E.
dc.contributor.authorWagner, A.
dc.contributor.authorHavránek, V.
dc.date.accessioned2022-01-31T11:00:32Z-
dc.date.available2022-01-31T11:00:32Z-
dc.date.issued2021
dc.identifier.citationMACKOVÁ, A. FERNANDES, S. MATEJÍČEK, J. VILÉMOVÁ, M. HOLÝ, V. LIEDKE, M. MARTAN, J. VRONKA, M. POTOČEK, M. BÁBOR, P. BUTTERLING, M. ATTALLAH, A. HIRSCHMANN, E. WAGNER, A. HAVRÁNEK, V. Radiation damage evolution in pure W and W-Cr-Hf alloy caused by 5 MeV Au ions in a broad range of dpa. Nuclear Materials and Energy, 2021, roč. 29, č. DEC 2021, s. nestránkováno. ISSN: 2352-1791cs
dc.identifier.issn2352-1791
dc.identifier.uri2-s2.0-85118541621
dc.identifier.urihttp://hdl.handle.net/11025/46702
dc.description.abstractČistý W a slitina W-Cr-Hf, které jsou perspektivními materiály pro jaderné fúzní reaktory, jako je DEMO, byly ozářeny při pokojové teplotě 5 MeV ionty Au2+ s dávkami mezi 4 × 10e14 a 1,3 × 10e16 ionty.cm-2 za účelem vytvoření různých úrovní poškození mřížky od jednotek až po desítky dpa. Odlišný charakter akumulace radiačního poškození, mikrostruktura a povaha defektů byly pozorovány u čistého W i slitin W-Cr-Hf, přičemž tyto slitiny vykazovaly zajímavou schopnost reorganizace poškození a snížení velikosti defektu při vyšších dávkách iontů, jak bylo stanoveno pozitronovou anihilační spektroskopií. (PAS). Vysoká míra radiačního poškození v ozařované vrstvě byla prokázána ve vzorcích W již při nižších dávkách Au-iontů ve srovnání se vzorky W-Cr-Hf, kde se poškození stupňovitě zvyšovalo s rostoucí dávkou Auiontů. Zřetelná akumulace defektů byla doprovázena odlišnou distribucí implantovaných Au-iontů v ozařované vrstvě stanovenou sekundární iontovou hmotnostní spektrometrií (SIMS), stejně jako tepelné vlastnosti ukázaly následné zhoršení hloubky v dobré shodě s Au koncentračními hloubkovými profily. TEM potvrdila výše uvedená zjištění, kde podpovrchová vrstva vykazovala po ozáření uvolnění defektů, maximum hustoty dislokační smyčky bylo identifikováno v hloubce podle predikovaného maxima dpa (posun částic na atom) pro nižší dávku Au-iontů. Kromě toho TEM ukazuje, že struktura pásu hustoty dislokací se objevila ve vzorcích W-Cr-Hf vykazujících pásmo defektů s vysokou hustotou podle projektovaného rozsahu Au-iontů současně s další vrstvou s většími izolovanými dislokacemi vyjádřenými ve větší hloubce jako rostoucí funkce dávky Au-iontů. Takový jev nebyl u W vzorků pozorován.cs
dc.format15 s.cs
dc.format.mimetypeapplication/pdf
dc.language.isoenen
dc.publisherElsevieren
dc.relation.ispartofseriesNuclear Materials and Energyen
dc.rights© authorsen
dc.subjectiontové ozáření W a slitiny W-Crcs
dc.subjectradiační poškozenícs
dc.subjectFúzní materiálycs
dc.subjectStrukturní analýza defektůcs
dc.subjectTepelné vlastnostics
dc.titleRadiation damage evolution in pure W and W-Cr-Hf alloy caused by 5 MeV Au ions in a broad range of dpaen
dc.title.alternativeVývoj radiačního poškození v čistém W a slitině W-Cr-Hf způsobené 5 MeV Au ionty v širokém rozsahu dpacs
dc.typečlánekcs
dc.typearticleen
dc.rights.accessopenAccessen
dc.type.versionpublishedVersionen
dc.description.abstract-translatedPure W and W-Cr-Hf alloy which are prospective materials for nuclear fusion reactors, such as DEMO, were irradiated at room temperature with 5 MeV Au2+ ions with fluences between 4 × 10e14 and 1.3 × 10e16 ions.cm-2 to generate various levels of lattice damage from about units up to tens of dpa. The distinct character of radiation damage accumulation, microstructure and defect nature have been observed in both pure W and W-Cr-Hf alloys, the latter exhibited interesting ability of damage reorganisation and defect size decrease at the higher ion fluences as determined by positron annihilation spectroscopy (PAS). High radiation damage rate in the irradiated layer has been evidenced in the W samples already at the lower Au-ion fluences compared to W-Cr-Hf samples, where the damage increased in steps with the increasing Au-ion fluence. The distinct defect accumulation was accompanied with the different Au-ion implanted distribution in the irradiated layer determined by Secondary Ion Mass Spectrometry (SIMS) as well as the thermal properties have shown the consequent worsening in the depth in good agreement with the Au-depth concentration profiles. TEM corroborated above mentioned findings, where the sub-surface layer exhibited defect release after the irradiation, the maximum of dislocation loop density has been identified in the depth according the predicted dpa (displacement particles per atom) maximum for the lower Au-ion fluences. Moreover, TEM shows the dislocation density band structure appeared in W-Cr-Hf samples exhibiting the high density defect band according the projected range of the Au-ions simultaneously with the additional layer with larger isolated dislocations pronounced in the higher depth as a growing function of Au-ion fluence. Such phenomenon was not observed in W samples.en
dc.subject.translatedW and W-Cr alloy ion irradiationen
dc.subject.translatedRadiation damageen
dc.subject.translatedFusion materialsen
dc.subject.translatedStructure analysis of defects, Thermal propertiesen
dc.identifier.doi10.1016/j.nme.2021.101085
dc.type.statusPeer-revieweden
dc.identifier.document-number718149900001
dc.identifier.obd43934570
dc.project.IDEF18_069/0010018/LabIR-PAV / Předaplikační výzkum infračervených technologiícs
Vyskytuje se v kolekcích:Články / Articles
OBD

Soubory připojené k záznamu:
Soubor VelikostFormát 
MARTAN_Radiation damage evolution in pure W and W-Cr-Hf alloy caused by 5 MeV.pdf9,42 MBAdobe PDFZobrazit/otevřít


Použijte tento identifikátor k citaci nebo jako odkaz na tento záznam: http://hdl.handle.net/11025/46702

Všechny záznamy v DSpace jsou chráněny autorskými právy, všechna práva vyhrazena.

hledání
navigace
  1. DSpace at University of West Bohemia
  2. Publikační činnost / Publications
  3. OBD